| Parameters | Units of Measurement | MicroConcrete LS | MicroConcrete HS | Patch Repair Mortar | |
|---|---|---|---|---|---|
| Flexural Strength | Mpa | 9.5 | 12 | 8 Mpa | |
| UV Stability | Stable/ Unstable | Stable | Stable | Stable | |
| Tensile Strength | Newton/m | 3.1 | 3.9 | 2.5 Mpa | |
| Compressive Strength | Newton | 50 | 70 | 38 Mpa | |
| Density | g/cc, Kg/m3 | 2297 | 2255 | 2111 | |
| Pot Life | Minutes | 60 | |||
| Warranted Life | Years | NA | NA | NA | |
| Type of System | Seamless/ Overlapped | Seamless | Seamless | Seamless | |
| Method of Application/Ease of Application | Easy, Moderately difficult, Difficult | Moderately Difficult | Moderately Difficult | Moderately Difficult | |
| Work Cycle | Fast/ Slow | Slow | Slow | Slow |